NI-Cr-based dental alloy for bridges and crowns
Composition: Ni 28%, Cr 22%, Fe 42%, Si 4%, Mo 3%, C, Mn, Cu
Melting temperature: 1330 - 1380°C
Melting point: 1260°C
Density: 7.8 g/cmc
Vickers hardness: 168 Hv10
Elasticity module: 205 Gpa
Presentation: 1kg